X-Ray inspection (at an angle, not top down) is tricky as the joints have no appreciable height. Absolutely no visual inspection is possible (unlike most BGAs, where you can see at least the outermost row). We also observed voiding under the prototype LGAs we assembled. I made sure that the board design was per the manufacturer spec and printed solder 1:1 with the pad and using our standard 2 mil reduction (1 mil on each dimension). Both soldered about the same, no difference in voiding.
Regards,
Amol
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Friday, June 19, 2009 9:22 AM
To: [log in to unmask]
Subject: Re: [TN] LGA assembly question
Hi Bev,
LGAs have higher standoff (solder pad contra board pad) and have a little
better signal integrity. If QFNs have any parameters better than LGA, I
don't know.
Normally, we do not make any other difference between them than solder
amount.
/Inge
----- Original Message -----
From: "Bev Christian" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, June 19, 2009 3:08 PM
Subject: Re: [TN] LGA assembly question
Sylvain,
Please enlighten us as to your understanding of the differences between
a QFN and an LGA.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Sylvain Kaufmann
Sent: Friday, June 19, 2009 9:06 AM
To: [log in to unmask]
Subject: [TN] LGA assembly question
Dear Technetters,
Our assembly workshop has to assemble 4 prototype boards where LGA
packages with 133 connections are used. I allready worked with BGAs or
QFNs but never with LGA packages and I am concerned about shorts/open
that could occur.
Provided that I cannot run tests and conditions are as followed:
- ENIG surface finish boards
- Vapor phase reflow soldering
- Pick and Place machine
- Leadfree or lead containing solder can be used
Would some of you be kind enough to share experiences/advices so that we
would have little chances to successfuly assemble these boards?
Thank you in advance for your help.
S. Kaufmann
************************************************************
Sylvain Kaufmann
CERN / European laboratory for particle physics Site de Meyrin
1211 Geneva 23
Switzerland
Dpt: EN-ICE-DEM (int mail J06600)
Phone: +41 22 767 37 02
Fax: +41 22 766 87 77
E-mail: [log in to unmask]
Web: www.cern.ch
http://cern.ch/dem
************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
WARNING: Export Control
This document may contain technical data within the definition of the
International Traffic in Arms Regulations (ITAR), and subject to the Export
Control Laws of the U.S. Government. Transfer of such data by any means to a
foreign person, whether in the United States or abroad, without proper export
authorization or other approval from the U.S. Department of State is
prohibited.
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|