Sat, 28 Jun 1997 13:41:29 -0400 (EDT)
Content-Type:
text/plain
Parts/Attachments:
text/plain (24 lines)
I believe it is most common to silkscreen legend after HASL.  Most legend
inks cannot withstand the thermal excursion without yellowing.   There is one
ink however, that will neither yellow nor pop off during HASL, and that is
made by Haven. 

I have run across one manufacturer that is applying legend before HASL using
this ink.  You would have to do tests to determine if this would work in your
facility.

Mark Dowding
Regional Technical Specialist
Insulectro

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2