Subject: | |
From: | |
Date: | Wed, 24 Jan 96 12:58:32 PST |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
contact your local pcb chemistry rep's for samples of the first part of
their two part solder strippers. they typically leave the copper/tin
intermetallics behind. don't know what to expect with gold.
______________________________ Reply Separator _________________________________
Subject: Sn-Pb etch
Author: [log in to unmask] at corp
Date: 1/24/96 10:58 AM
Can anyone recommend a method to completely remove the 63-37 solder from a
surface, leaving the underlying intermetallics untouched? I have tried
hydrochloric acid; it works for solder reflowed on Cu, but in joints with
gold it apparently re-precipitates gold artifacts. Any help would be
greatly appreciated.
Edwin Bradley
Motorola
|
|
|