Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Thu, 25 Jun 1998 14:04:04 -0600 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Hi all,
I have a few questions like to get the answer from the expertises:
1. Nitrogen being used on the wave process, what kind of process
improvement do we achieve? I heard people said that they have better
joint, better reflow.....
2. If it helps to reduce drossing of solder, how much solder do we save
monthly? How much dross produce/reduce each month? (Use % for
calculation).
3. How much nitrogen consumption in a month? (Let's say the machine runs
2 shifts in 22 days/month).
How can I measure/justify of using nitrogen in the process in terms of
quality and savings?
Your answer would be a great help for me.
Thanks
Simon Shin
> ----------
> From: superflx[SMTP:[log in to unmask]]
> Sent: Thursday, June 25, 1998 1:19 PM
> To: [log in to unmask]
> Subject: Re: [TN] Nitrogen in the wavesolderingproces
>
> If you use a No-Clean flux with clean, fresh components and new HAL or
> OSP boards, the nitrogen will add, marginally, to the process. If you
> use a water-soluble flux, the nitrogen does not add anything as the
> flux will overcome any oxidation problems.
> Our experiuence has been that Nitrogen doesn't necessarily add
> anything to the soldering process, but helps reduce drossing of
> solder. If reducing dross can help save money relative to the cost of
> nitrogen, then its a worthwhile investment.
> Phil
> Jesper Kjærnulf Konge wrote:
> At our factory we are going to have a new waesolderingmachine
> with nitrogensupport. But our director dosen't think that we need the
> nitrogen because it has no effect compared to the price that we have
> to pay. But in me department we dosen't aggree. I would like to hear
> about your experience with nitrogen so that we can tell our director
> that it isn't just us that thinks that nitrogen soldering is good. And
> if anyone has a meaning about the Seho MWS-8200 PWR i would like to
> hear that too. With Regards Jesper KongeDanica Supply A/SDenmark Mail
> : [log in to unmask] <mailto:[log in to unmask]>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|