FL- Fiberglass Laminate
GE- Glass Fabric base, Epoxy resin, General purpose
0.10- Nominal Thickness
C-Copper
1/0- Nominal Foil Thickness
B-Grade of Pits and Dents
11 or II- Believe this should be Class 2 of Thickness Tolerances
Hope This Helps
Roger Tingler
Methods Engineer
Colonial Circuits
V:800-578-9602 x102
540-752-5511x102
F:800-631-0856
540-752-4832
E-mail: [log in to unmask]
"This document or these discussions contain(s) technical data under U.S.
Government export control regulations, (ITAR) 22 C.F.R. Parts 120-130, or
(EAR) 15 C.F.R. Parts 730-774. Transfer of information in this document by
any means to a foreign person or entity, whether in the U.S. or abroad,
without appropriate export authorization, is prohibited and may result in
substantial penalties."
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Hodge
Sent: Tuesday, December 20, 2005 2:02 PM
To: [log in to unmask]
Subject: Re: [TN] <List>Re: [TN] MIL-P-13949 question
1/0 is single sided 1 ounce copper. BII or B11? I am not sure
At 12:00 PM 12/20/2005, you wrote:
>FL, Fiberglass Laminate
>
>No clue on the 0B11
>
>Sorry!
>
>Deac
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin Asbell
>Sent: Tuesday, December 20, 2005 1:48 PM
>To: [log in to unmask]
>Subject: [TN] MIL-P-13949 question
>
>Have a question on a laminate designation in a fab drawing, the following
is
>exactly how it is spelled out;
>
>MATERIAL: LAMINATED GLASS EPOXY SHEET, COPPER CLAD PER MIL-P-13949 FL-GE
0.1
>C1/0BII.
>
>The fab drawing depicts a board with top and bottom copper.
>
>It is the FL and the 0BII that I'm puzzled over, anyone have thoughts???
>
>
>Thanks,
>
>Franklin
>
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|