If the solder pallets are titanium then you should wash them in a detergent
(to remove any oils) then bake them in the oven to reoxidize the titanium.
(this will prevent solder from sticking to the freshly machined titanium).
Nice thing about molten solder is that it doesn't get contaminated easily
(except by metals). Nearly all contaminates float to the top. Even tools
you drop in it. (not recommended)
You will want to clean off any oils which will contaminate the product or
the flux. Oils will also burn on to the pallets making them look awful
(forever).
So no metal chips and no machining oils.
Hope this helps
Russ
-----Original Message-----
From: (No Name Available) <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Thursday, November 05, 1998 5:42 PM
Subject: [TN] Cleaning Solder Pallets
>I've modified several wave solder pallets for a customer, besides blowing
off
>the lose material how should I clean them, so not to contaminate the
solder.
>
>Thanks in advance,
>
>Kevin Willis
>Advantage Tool & Microweld
>Decatur, Al.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|