TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Date:
Wed, 28 Aug 1996 16:33:48 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (12 lines)
Read the paper presented in E.P.&P. -"Matte Surface Solder Masks Reduce
Solder Ball Defects", June 1993, pp58-60

***************************************************************************