Hi technetters:
The "skiops" in Spray coating are mostly a function of the resist. Percent
solids, thixotropic index and wetting agents all play a roll. Some
adjustments can be made by adjusting atomization and pressures on the
equipment. Diluting the resist with too much solvents can also result in
"skips"