Phil,
It does not include vibration but just temperature cycling.
regards - wee mei
"Crepeau, Phil" wrote:
> hi,
>
> did your ess include vibration? i've seen fasteners fail, and the subsequent fretting in vibration caused a 'dirty' appearing surface.
>
> phil
>
> -----Original Message-----
> From: fullname [mailto:[log in to unmask]]
> Sent: Tuesday, September 25, 2001 12:34 AM
> To: [log in to unmask]
> Subject: [TN] Dirt on Coated Board (UC)
>
> Some assembled boards were coated with Humiseal 1B31. After the ESS
> tests at 110 degree C, dirts were found on the board and component
> surfaces on both sides. I have checked the data specification on 1B31
> and found that under cured enivronemnt, the coating should withstand -65
> to +125 degree C.
>
> Can someone advice me what could be the cause of this problems?
> Your assistance is greatly appreciated.
>
> Regards - Wee Mei
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|