Lou:
What solder mask are they having adhesion problems with and what is
the surface that they are proposing to put the oxide on?
______________________________ Reply Separator _________________________________
Subject: Black oxide on outer layers
Author: [log in to unmask] at corp
Date: 9/25/96 12:37 PM
Greetings !
The Fab house that we use has recently asked us if they could use a black
oxide treatment on external layers of our designs. I know that this process
is used for internal layers but I want to know if any of you have used it
for external layers ? Their reason for using it is " To create better
adhesion for the solder mask and eliminate potential slivers ". To me, this
sounds more like a process problem. What do you think ?
To recap, do any of you use a black oxide coating on outer layers ? If so,
why ?. If not, why not ?
Thanks in advance for your help !
Lou Takach
Union Switch & Signal Inc.
412.688.2574 (voice)
412.688.2399 (fax)
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|