Hi Amol!
The part cab only absorb moisture at a certain rate because of the
density of the body material, therefore going through an aqueous wash
isn't going push the moisture into the die cavity (which is what you're
worried about), any faster than if it were sitting out on the floor in a
humid environment in an unsealed bag...at least that's the way I
understand it.
I've never baked a double-side board with MSD's after aqueous wash
before I built the second side, as long as I was in the floor life
window for the moisture sensitivity level of the part, and I've never
had a problem whatsoever.
-Steve Gregory-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
Sent: Wednesday, September 06, 2006 12:18 PM
To: [log in to unmask]
Subject: Re: [TN] Populated board bake out after 1st side reflow/DI wash
Okay, I am intrigued, what is the difference between the moisture
absorbed over time and the moisture (water) absorbed in the aqueous
wash?
Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing, Inc.
941 Route 38 Owego, NY 13827
Phone: (607) 687-7669 x349
Fax: (607) 687-9733
[log in to unmask]
www.harvardgrp.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, September 06, 2006 1:07 PM
To: [log in to unmask]
Subject: Re: [TN] Populated board bake out after 1st side
reflow/DI wash
Hi Joe!
Going through a aqueous cleaner won't cause problems with 2nd side
reflow. The moisture that you have to worry about is the moisture that
is absorbed over time. Sticking to the floor life time guidelines that
go along with the limits of each part, i.e.; Level 1, 2, 3, etc., is
what you need to be concerned about. You don't need to re-bake the
assemblies if you're within the floor life of the part.
-Steve Gregory-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Macko, Joe @ IEC
Sent: Wednesday, September 06, 2006 11:31 AM
To: [log in to unmask]
Subject: [TN] Populated board bake out after 1st side reflow/DI wash
Fellow techs,
Hello.
A general question came up about the need to re-bake a double sided
board after 1st side reflow/DI wash before starting 2nd side assembly.
The concern is that the board (or mounted MSDs) may absorb enough
moisture going through the high-pressure DI water in-line cleaner to
potentially cause a problem during 2nd side reflow. There are some MSDs
mounted on the 1st side but both sides are assembled before exceeding
any of the component's floor life. It has been suggested that some level
of bake out should be performed after 1st side cleaning to prevent
potential problems during 2nd side reflow but the push back is that this
adds cost, handling, etc... that may introduce its own associated
problems and is not really necessary.
Thanks again. It is great to have a knowledgeable forum such as TechNet.
Joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|