Pat, like Jerry Cupples, I was not able to contact you directly.
I have been trying to set up a cross-section lab, too.
Buehler has a toll free number, 800-BUEHLER.
Another possiblity is MARK V Laboratory in East Granby, CT.
800-243-9776. This company has its own line, and can get rebuilt equipment.
Please contact me directly for more information.
Lou Hart 412-858-6117
.
***************************************************************************