Bev,
One of the reasons there isn't a specification for gold plating thickness on component leads is because solder assembly engineers would like it to be zero and the packagers doing internal wire bonding would like it to be a couple of hundred microinches thick. Most packages I've come across have 150 +/- 50 micro inches of gold
Regards,
George
George M. Wenger (908)-546-4531
Reliability Engineer
RF Power Amplifier Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059
[log in to unmask]
-----Original Message-----
From: Dave Hillman [mailto:[log in to unmask]]
Sent: Wednesday, August 06, 2003 1:40 PM
To: [log in to unmask]
Subject: Re: [TN] Gold thickness
Hi Bev - if you find a specification that defines the gold plating
thickness let me know - I have also searched but have come up empty. Some
of the component fabricators can not even tell you if a component will have
gold or tin/lead as their manufacturing locations are setup for one or the
other but not both finishes. Sometimes an internal specification can add
some predictability but not always. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Bev Christian
<[log in to unmask] To: [log in to unmask]
ET> cc:
Sent by: TechNet Subject: [TN] Gold thickness
<TechNet@listserv
.ipc.org>
08/06/2003 10:23
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Bev
Christian
TechNetters,
I have checked the archives and can find no answer to this question. Is
there a standard (JEDEC, IEC, etc.) for gold thickness ON COMPONENT leads?
I am NOT asking about boards. Thanks.
regards,
Bev Christian
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|