     You can dunk it in sulfuric acid and touch the chrome with a bar of 
     zinc metal or add thiourea to etch the chrome.
     
     Aric Parr
     United Technologies Electronic Controls


______________________________ Reply Separator _________________________________
Subject: Re: FAB: to etch chrome but not copper
Author:  [log in to unmask] at internet
Date:    8/1/96 7:59 PM


     RE: Etching chrome.  As an unspecific recollection, I believe that a 
     KOH + Potassium Permanganate solution will strip Chrome from Copper. 
     I am not certain of concentrations and temperatures.  Note that this 
     will create environmental concerns on the spent etch solution and 
     rinses.
     
     Marshall Gurian
     Coates ASI
     
     
______________________________ Reply Separator _________________________________
Subject: FAB: to etch chrome but not copper
Author:  [log in to unmask] at internet 
Date:    8/1/96 11:52 AM
     
     
Can anyone tell me what etchant will dissolve chrome but not copper?
     
I'm thinking about using cold dilute sulfuric acid but I'm not sure what is 
used commercially anymore.
     
Thanks!
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************
     
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************