Double check following.....
1. AC ripples in current ..
2. Color of film on anode..
3. Analyse film of anode..
4.Contaminated brighner..
5. Unbalanced components of brightner.
6. Quality/ Tracibility of anode lots
7 Cheaper anodes..
8. History of tank solution
9. Lot more reasons...