From: Jeannie Newhart
Subject: Test Data for GETEK
GE Electromterials has done extensive testing on GETEK laminate at 1MHz-15GHz.
This data includes Dk and Df at various frequencies over temperature and
humidity for specific core thicknesses. Please contact me for more
information.
Regards, Jeannie Newhart Market Development West/GETEK