Dear sir,
Please try Minico M-7200 of Emerso&Cuming, it proof to 240 C HASL and 260
C Solder heat resistance. The branch in Asia-Pacific is in Japan
100 Kaneda, Atsugi-shi
Kanagawa-ken, 243
Japan
Tel : (81) 462-25-8815
Fax : (81) 462-22-1347
Good luck
Noppadol S.
At 10:06 17/6/98 +0500, you wrote:
>Dear Sir,
>
>We are the largest manufacurer of printed circuit board in INDIA .
>
>We have the fallowing requirement of peelable SM.
>
>We want Peelable SM ink that with stands IR Relow & Wave soldering cycles.
>
>IR Reflow means board temprature upto 240 deg,c for 40-60 secs
>
>
>wave soldering means a wave of 250 Deg c and pre heat of 150-200 DEG C.
>
>Our exisiting peelable inks of two suppliers withstands only 210 DEG c
>
>Can any one suggest us a good peelable ink source?
>
>
>
>Awaiting yr reply
>
>
>
>Regards
>
>
>
>L.VINOD PH: +91-8221-26375,
>26618
>INDAL ELECTRONICS LTD., FAX: +91-8221-26641
>PLOT NO 12A, INDUSTRIAL AREA WEB: http://www.indalpcb.com
>NANJANGUD, MYSORE DIST., E-MAIL : [log in to unmask]
>KARNATAKA - 571 301.
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|