Are We Having
Fun Yet? RE>Nailheading
The issue of nailheading has also been resolved in the new mil spec ntended to
replace MIL P 55110, and nailheading is not cause for rejection in MIL PRF
31032.
Lisa Greenleaf
|
|
|