I would like to get some information on expected yields for
non-soldered leads using 240 pin PQFPs.5mm pitch. Our
yield is 25% or more bad circuit cards on average. The lead
coplarity ranges from 0 to 3.5 mils with most falling in at 2.5
to 3.5 mils. Is this common or can process improvements
without equipment purchases help?. We have a FUJI GSP III
screen printer with rubber squeezes and are using 7 mil thick
laser cut stencils. I could use any help and expected yields
information. We are going to change to BGA sometime later
this year.
Thanks
Ron Mowbray
Menber of Technical Staff
Paradyne Corp.
Largo, Fl.
e-mail: [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################