Not by design Doug. If you have exposed planes then there may be
justification, but since coating only really prevents leakage due to
condensation, the fact that it isn't there makes no difference as far as
I can see
Regards
Ian Fox
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: 20 October 2010 19:21
To: [log in to unmask]
Subject: [TN] Conformal Coating Board Edges
Good afternoon all,
I am glad we all appreciate Inge and the time he puts into making this a
fun and interesting forum. To sum up: Ditto.
I have a question related to conformal coating, a sort of survey. For
those of you that conformally coat your assemblies, do you coat the
edges of the boards? Why or why not?
There is an internal debate here and I wanted some other viewpoints
before offering my own.
Doug Pauls
Rockwell Collins
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
--------------------------------------------------------------------------
This message (and any attachment) is confidential and is intended for the named recipient only.
If you receive it in error please e-mail back the sender and permanently delete the original message and any copies.
Rolls-Royce Goodrich Engine Control Systems Limited.
Registered Office: Moor Lane, PO Box 31, Derby, DE24 8BJ.
Registered in England No. 06686268.
--------------------------------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|