We had a big bang problem with SMT tantalum caps let me tell
   you about it.      The application of the tant was bottom side assy
  which went through a wave solder.   Normal process of 260deg C
  the dwell times were fine and all that.  It is a no clean process so
  aqueous cleaning was not an issue.   During our Gen Rad testing
  the tants were Bang-ing.    Why?    So we beat up the manufacturer.
  Isn't that always the thing to do?   Well what we found out-during my
  visit to the vendor was this.   Tantalums hate thermal shock.   When
  we explained our process the vendor said, "Oh I see.  So you don't
  believe in pre-heat before subjecting these tiny little parts to a temp
  of 500degsF!!!

  We changed our process to a moderate pre-heat and ba-da-bing,
  No more failures.    I'd say check your process.

  Don Fumia

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2