> And another:where does the lead carbonate come ?
>
>
Lead oxidizes to Lead Oxide, or Lead Hydroxide, (Lead Hydroxide = Lead Oxide
+ Water) then reacts with either Carbon Dioxide in the air (suspect less
likely) or with Carbonates in water (suspect more likely) and Bingo!
***************************************************************************