As long as the oven can provide the thermal profile you need, I don't think
size matters. Just check all areas of the board for adequate temperature.
Sticking a large cold mass into a small oven will drag the profile down,
and the oven may take a longer time to compensate for this than it would
for a relatively smaller mass. If you have a large volume of work, a larger
oven might be justifiable in terms of having a larger "heat pool" that
won't be dragged down so much by relatively smaller boards. It will be more
stable thermally speaking and will probably recover its temperature more
quickly than a small oven.
My hypothetical 2 cents.
Peter Duncan
Dave Snyder
<[log in to unmask] To: [log in to unmask]
COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST
Sent by: Aero/ST Group)
TechNet Subject: [TN] Reflow Oven Sizes
<[log in to unmask]
ORG>
11/06/01
01:04 AM
Please
respond to
"TechNet
E-Mail
Forum."
What advantages does a larger reflow oven have over a smaller one other
than
size? We have a small unit that will fit a 10" wide board. We would like a
unit that would fit a 13" wide board. Is there any other justifications to
a
larger oven? We do not use lead free.
Thanks
Dave Snyder
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|