Gary,
You might try putting the AXAREL 2200 in a machine specifically designed for
removing misprinted solder paste (Electrovert and several others make these
for 10's of thousands of dollars which is less than $1,000,000!).
Alternatively, you may want to try a couple of Petroferm's other products --
BIOACT SC-10 and BIOACT SC-22. Please reply if you would like more
information.
Beth Bivins
Petroferm Inc.
904-277-5236
[log in to unmask]
***************************************************************************