TECHNET Archives

June 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Thu, 13 Jun 2013 14:31:39 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (43 lines)
There you go, Joyce. Had not thought of that.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Thursday, June 13, 2013 9:25 AM
To: [log in to unmask]
Subject: Re: [TN] Titanium

Silk screen. TiO2 white color filler. 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Amol Kane [mailto:[log in to unmask]]
Sent: Thursday, June 13, 2013 10:03 AM
To: [log in to unmask] <[log in to unmask]>
Subject: [TN] Titanium

Dear Technetters,
We are seeing some titanium residues (confirmed by EDX) on solder joints after wave soldering post wash (that is not to say they are not present post wave, more analysis is ongoing). Water soluble process, high lead alloy, and a saponified wash. So far the Ti residues are only detectable on the solder joints, not on the assy surface. For general information. what are some possible sources of Ti on the assembly?

Regards,
Amol



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2