We currently process core boards with vias in the surface mount pads.
Parts are soldered directly over the filled vias with plating and
solder over the vias.
Roxanne Tovey
______________________________ Reply Separator _________________________________
Subject: Re: via holes & surface mount components
Author: [log in to unmask] at esdigate
Date: 2/13/96 10:39 AM
Via hole should be atleast .025 away from surface mount pads.
______________________________ Reply Separator _________________________________
Subject: via holes & surface mount components
Author: [log in to unmask] at corp
Date: 2/12/96 4:10 PM
What is the minimum distance via holes can be to surface mount components?
|
|
|