Just the one assy. of five. The last one, which was delayed because I broke a
VERY expensive fiber optic cable. I tried a little experiment last night.
Used new copper and treated it with the chemicals we use. The WS flux did
turn green but not quite the same color. Seems odd though that the residue is
on parts that were pasted and reflowed and washed several time. It does not
appear on the parts that were hand soldered and manually cleaned.
Thanks for putting the pics up. Be sure to take them off in a couple of days.
Don't wanna load up your site. I am trying to get our network guys to set up
something so I can post pictures too.
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Wednesday, May 05, 2004 9:47 AM
To: [log in to unmask]
Subject: Re: [TN] Green residue.
Hi Charles!
Finally got your pictures up. Go to: http://www.stevezeva.homestead.com and
look at "Green Residue 1 and 2". Looking at the pictures, it sure looks like
something is reacting with the copper. Maybe some flux got accidently
splashed
or spilled on the board after it was cleaned. How many assemblies exhibit
this
problem?
-Steve Gregory-
> When we do the hand solder it takes about 1.5 hr. so we clean with IPA then
> wash with water. The flux core is alcohol based and cleans fairly well with
> IPA but we do hand clean after with saponifier and water. I did a little
> experiment with new copper. It looks like it might be the WS flux, but the
> parts that have the green are not hand soldered and the parts that are hand
> soldered do not have it.
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|