Subject: | |
From: | |
Reply To: | |
Date: | Sat, 11 Mar 2006 06:31:52 -0500 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
March 11, 2006
We have used silver coated stranded wire for many years with no known problems in a military application. The IPC repair standard IPC7711/7721A also has same caution note.
----- Original Message -----
From: Jones, Evamaria<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Thursday, March 09, 2006 3:20 PM
Subject: Re: [TN] Jumper Wires
Steve,
IPC-HDBK-001 section 5.0.5, Silver Coated Leads, pg 56 states that silver finished leads (solid) are not typically used because of silver migration (silver/tin intermetallic) which can cause solder joint failure.
Evamaria Jones
General Dynamics
Quality Engineer
Instructor
________________________________
From: TechNet on behalf of Vargas, Stephen M
Sent: Thu 3/9/2006 10:10 AM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: [TN] Jumper Wires
All:
We need to add a 30 AWG jumper wire to a lead-free assembly (Class
II). IPC-A-610 says that silver plated stranded wire should not be used
due to possible corrosion under certain conditions. Our thoughts are
that this (corrosion possibility) is unique to stranded wire. Would
silver plated solid wire be an alternative? Any input would be
appreciated. Thanks.
Regards,
Steve Vargas
Sr. Mfg. Engineer
Polaris Contract Mfg. Inc.
[log in to unmask]<mailto:[log in to unmask]>
508-748-3399 ext.192
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|