Subject: | |
From: | |
Date: | Thu, 19 Jun 1997 07:18:31 -0400 (EDT) |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
As a large supplier of tin strip chemistry I can tell you that your nitric
chemistry should hold about 150g/l tin, 20g/l iron, and 10g/l of copper. The
chemistry should not contain any chelaters and most large customers simply
bleed this into their non chelated metal bearing waste streams. A tin strip
consumption of 1 drum a day would mean that you would only need to feed 2
gallons an hour to your waste stream. This dilution is usually helpful.
I would check the level of copper in the spent chemistry and if it is over
12g/l you are etching excessive amounts of copper. The etch rate on a broken
in bath should be only 10 - 15 millionths/ minute.
Regards,
Chris McGary
Dexter Electronic Materials
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|