See below Bill
Bruce Stilmack
GDLS-TO Manufacturing Engineer
(850) 574-4773
[log in to unmask]
"Kasprzak, Bill
(sys) USX" To: [log in to unmask]
<[log in to unmask] cc:
OM> Subject: Re: [TN] RE : [TN] SN63
Sent by: TechNet
<[log in to unmask]>
07/28/2004 10:24
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
"Kasprzak, Bill
(sys) USX"
Please excuse my ignorance on the issue of Sn63 as it relates to Military
and Space hardware but, has it been decided which alloy is going to replace
Sn63? - No, there is no drop in replacement that I know of at this date
Will there be a carte blanche approval on all military programs to switch
to
a new alloy without the benefit of qual testing? (I doubt it, who is going
to pay for this testing?)- Again, there is no firm DOD direction that I
know of at this date. If I am wrong, I'd love to hear the answer.
If lead free applies to only future procurements, when is the future? - The
future is now. As new designs come into being, it appears the direction is
going to be lead free. And this doesn't just mean lead free. The wording
is actually no "hazardous" material. Cadmium is also banned.
Is FCS a single program or a directive for future programs? - FCS is a
single program now under design and prototyping. It is the next step the
Army wants to take in light mobile systems. However, other programs I have
seen that are going through the development phase are also being directed
towards no hazardous material.
The way I see it, it's going to be a long time before mil programs adopt a
new lead free alloy. I can't imagine a EU country not purchasing military
hardware due to a lead free clause. - Can't answer that.
Do I need to start thinking about having dual capabilities for leaded and
lead free programs? I'm feeling any pressure to do so at this time but
maybe
it's more imminent than I thought. Again can't answer, though I will tell
you that I believe the move is legitimate enough that I am looking to
purchase a new dual wave system.
Any advice from the "big guns" out there?
Bill Kasprzak
Moog Inc., Systems Group, Process Engineer
-----Original Message-----
From: Bruce D Stilmack [mailto:[log in to unmask]]
Sent: Wednesday, July 28, 2004 9:54 AM
To: [log in to unmask]
Subject: Re: [TN] RE : [TN] SN63
Remember, Ramon said "In the military circles that I know about", the new
Army programs like FCS (Future Combat Systems) at present are supporting a
no lead requirement.
Bruce Stilmack
GDLS-TO Manufacturing Engineer
(850) 574-4773
[log in to unmask]
David Suraski
<dsuraski@AIMSOLD To: [log in to unmask]
ER.COM> cc:
Sent by: TechNet Subject: Re: [TN] RE : [TN]
SN63
<[log in to unmask]>
07/28/2004 09:50
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to David
Suraski
Isn't military outside the scope of RoHS?
-----Original Message-----
From: Brian Ellis [mailto:[log in to unmask]]
Sent: Wednesday, July 28, 2004 9:48 AM
To: [log in to unmask]
Subject: Re: [TN] RE : [TN] SN63
Cheeky question: Does this mean you won't be selling any of your military
hardware to the EU or for use in California? :-)
Brian
Dehoyos, Ramon wrote:
> In the military circles that I know about there is no intentions
of changing from SN63. It will be used for a long time . Lead free solder
will create problems and not benefit society as it is being sold.
>
>
>
>
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Eric Laroche
> Sent: Wednesday, July 28, 2004 8:04 AM
> To: [log in to unmask]
> Subject: [TN] RE : [TN] SN63
>
>
> Morning All,
>
> Maybe they are reffering to the price increase that was seen in the
> last year....% wise it has gone up quite a bit.
>
> Regards,
>
> Eric
>
> -----Message d'origine-----
> De : TechNet [mailto:[log in to unmask]] De la part de David Suraski
> Envoyé : 28 juillet, 2004 07:43 À : [log in to unmask] Objet : Re: [TN]
> SN63
>
>
> Kenny,
>
> Tell them to come to us - we'll sell them all the Sn63 they can handle!
>
> Seriously, as a solder manufacturer I've seen absolutely no shortage
> of Sn63. I'm really surprised to see this comment.
>
> Regards,
>
> David Suraski
> AIM
> +1-401-463-5605 ext. 5210
> www.aimsolder.com
>
> -----Original Message-----
> From: Bloomquist, Ken [mailto:[log in to unmask]]
> Sent: Tuesday, July 27, 2004 5:54 PM
> To: [log in to unmask]
> Subject: [TN] SN63
>
> We have a couple of CM's that are telling us that they are having a
> hard time getting SN63 for their wave solder and hand solder. We've
> used it for a million years and I can't believe that the industry is
> no longer going to make SN63 as a common solder.
>
> Maybe I've been living under a rock up here in the Great Northwest but
> is anyone else seeing this as an issue?
>
> Thanks,
>
> KennyB
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|