Jim,
we use Rogers TMM since some years. Optiprint in Switzerland make them for us and we have only found one problem : they may be a little different for wire bonding. We are just a small user of TMM. / Ingemar
Good afternoon, Technet...
We're considering using Rogers TMM-6 material for an RF design which would
include multilayers (4) of TMM and multilayers (4) of Polyimide with both blind
and through vias. Does anyone, preferably both fabricators and assemblers,
have any experiences with this material? Any fab or assembly problems? Please
advise...
Thanks,
Jim Marsico
AIL Systems Inc.
(516) 595-5879
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|