Robotic Process Systems makes a nitrogen nozzle for its solder pots as well.
We tell our customers to soak them in a bucket overnight in a solution that
will break down what ever type of flux you are using. Then bubble compressed
air through them until the membranes are cleared. If you still have vapor
degreasers (he looked back fondly) this is(was) the best method.
DO NOT USE ANY TYPE OF METAL BRUSH OR WIRE WHEEL!!!!!!!! This will cause the
pores to close and then you will be buying another manifold set.
################################################################