> Good day to all,
> I have experienced the effects of sunken solder after the PCB passed
> through the Wave Soldering Machine. The solder is always sunken at the
> interface between a connector and the PCB, but other areas are well formed.
Are the holes for the connector too large? They probably need only be 0.4mm
greater than the width of the connector pin.
--
Regards, JNA Telecommunications Limited
___ _____ 16 Smith Street
Dom Bragge (VK2YAK) __ / / |/ / _ | Chatswood NSW 2067
PWB Designer / // / / __ | AUSTRALIA
Tel: (+61 2) 9935 5792 \___/_/|_/_/ |_|
Fax: (+61 2) 417 3862 http://www.jna.com.au
|
|
|