Ted,
We have used Circuit Repair Corp.; 108 Turnpike; Rowley, MA 01969; 508/948-7973
for FR4 repairs. We have been very happy with their work.
They tell me that they do Teflon too, but we have no experience there.
Good luck
Charlie B.
To: TechNet @ ipc.org ("[log in to unmask]") @ Internet
cc: (bcc: Charles Barker/IO-US)
From: Ted.A.Edwards @ CAS.honeywell.com ("Edwards, Ted A (AZ75)") @ Internet
Date: 05/08/96 12:21:54 PM
Subject: ASSY: Teflon Board Repair
Occasionally with Teflon base material boards adhesion of a pad or run
is lost during assembly, especially with connectors and larger parts which
require more heat, and we are wondering if anyone has experience in rework
or repair to reattach pads or runs to Teflon boards. We would like bond
strength in the range of original and without microwave performance
degradation. Anybody got any ideas or suggestions?