Frank,
Don't do it!
FR2 and SMT are not a good mix.
I only use FR2 on small thru hole PCBs.
I fear you will have serious yeild problems that would cost considerably more
than FR4 will. FR2 will warp considerably and cause component level problems
after reflow.