Ioan,
From the replies, all of the X-Ray machines out there are great. For my
money, I like the X-Tek (at previous company we bought one X-Tek, and then
bought a second and placed at our contract manufacturer). During
evaluation, I looked at Dage, Phoenix, Fein Focus, and X-Tek and all work
well.
I highly suggest spending a day on each machine so you can compare for
yourself (ease of use, image quality - both live and captured, analysis
tools, etc). Also, all of the manufacturers can give you contacts of
people who have their equipment. Give calls, ask questions.
Good luck.
Al Kreplick
Sr. Manufacturing Engineer
Circuit Card Assembly
Air-toAir/Precision Strike/Land Combat
Raytheon Integrated Defense Systems
978-470-9931office
978-245-1702 pager
978-470-4307 fax
[log in to unmask]
Ioan Tempea <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/15/2008 08:55 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ioan Tempea <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] X-Ray equipment
Dear Technos,
One more topic: what are your experiences with X-Ray equipment? Which
brand/model would you recommend or not advise?
We are a typical EMS and would like to inspect as accurately as possible
BGAs and leadless. So voids and hole-fill measuring capability is
desired. If possible, we would like to be able to localize an open BGA
joint.
Not exactly looking for big budget laminography machines like the 5DX,
but it should at least be 2D plus rotation capability. Or a regular, not
so loaded 3D system...
On-line and off-line answers welcome.
Thanks,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|