Amol,
Do you use titanium wave solder pallets? If so, are they cleaned in the same machine you use to clean your assemblies?
Leland
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
Sent: Thursday, June 13, 2013 10:04 AM
To: [log in to unmask]
Subject: [TN] Titanium
Dear Technetters,
We are seeing some titanium residues (confirmed by EDX) on solder joints after wave soldering post wash (that is not to say they are not present post wave, more analysis is ongoing). Water soluble process, high lead alloy, and a saponified wash. So far the Ti residues are only detectable on the solder joints, not on the assy surface. For general information. what are some possible sources of Ti on the assembly?
Regards,
Amol
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
________________________________
“Confidentiality Notice:
This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments.”
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|