now things are getting very interesting: It does not appear to be the same
V200 stuff based on Brain and Phil's discription. I don' t use the stuff.
Is it possible for Euro guy and US guy put a strip of pH paper in the V200
and see if there is any difference... may be the V200 changes when shipped
across the ocean...the pH level is depend upon which side of the road you
drive ("do not add saponifier to the country drive on the right side, just
add saponifier for the lefties..." sorry, sorry, the imagination get out of
control without any saponifier)...
jk ;-)
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of b_ellis
>Sent: Friday, August 09, 2002 4:22 AM
>To: [log in to unmask]
>Subject: Re: [TN] Cleaning Solvent for Military Product
>
>
>It would seem that there is either mis- or dis-information on the go.
>Firstly, I reproach Zestron for an uninformative website. Most companies
>put technical details and MSDS on their site.
>
>OK, here goes: if Vigon were just an alcohol and water, why does the
>solution have a pH exceeding 11? There is no way this could happen. I
>have not seen a US MSDS but if it does not mention that it contains an
>amine, then either the European product is different from the US one
>(this is unlikely with an identical designation) or it is sadly lacking
>in important information. Just dip a pH indicator paper into the
>solution and then believe me!
>
>All saponifiers contain an alkaline product, most frequently an organic
>amine. This is no exception, but I forget which one is used in Vigon. It
>may be a derivative of one of the propylene amines. It may be that the
>MSDS uses a synonym that disguises tha amine group with something
>containing nitrogen (analogue to ammonia = nitrogen trihydride): that I
>cannot say. In any case, the odour of the hot solution gives the amine
>away to anyone who has experience of using them. Commercial defluxing
>saponifiers also contain solvents, because not all the flux residues are
>saponifiable and solvents are a requirement to ensure maximal cleaning.
>They are usually either heavy alcohols or diglycol ethers or a
>combination of both. Therefore it is normal that the MSDS should mention
>them.
>
>Still don't believe me? OK. Look up the Handbook of Solvents, edited by
>George Wypych, Chemtec Publishing (2001), p. 899, Section 14.8.2.1.4,
>entitled Water-based cleaning agents based on MPC technology. This
>section contains the following sentence: "Alkaline pH, that is essential
>for the saponification process, can be realized through biochemical
>buffer systems, predominately aminoalkanoles." And that was not written
>by Brian Ellis but by Martin Hanek of Dr O.K. Wack Chemie and Andreas
>Mühlbauer of the Zestron Corporation. Straight from the horse's mouth,
>n'est ce pas? Or, rather, nicht war? Incidentally, the terminology in
>this sentence is questionable: there is nothing bio- about the
>buffering.
>
>Worker safety: it is essential that operators wear full chemical
>protection when handling either the concentrate or the working solution.
>An untreated splash of the concentrate, or even the solution, in the
>eyes could lead to rapid blindness. At the best, even if treated
>immediately, it would be screamingly painful. It should never be used or
>stored without a functional eyewash basin in the immediate vicinity. The
>skin is also sensitive and splashes should be washed immediately in
>copious rinses (if I clean one circuit by unprotected hand in the
>solution with a brush, the skin desquamates from that brief exposure -
>voice of experience). Vapours: all amines are toxic to inhale. I don't
>know the OEL for this particular one, but MEA, the most popular amine,
>is usually in the 3 - 10 ppm range, in most countries. If you can smell
>it, the concentration is probably already too high. For example, in the
>US, the PEL for MEA is 3 ppm and the odour threshold is 2.6 ppm.
>Although I don't have figures, there is no reason to believe that other
>amines are that much more benign. Also, if ingested, it would not
>improve the health of the operator. Large quantities of lemon juice (or
>Coca Cola), followed by a suspension of active carbon in water, would be
>the best treatement if the patient is conscious. Do NOT provoke
>vomiting. Call a doctor immediately. If the patient is unconscious, keep
>airways free, monitor his state and if necessary administer oxygen or
>mouth-to-mouth respiration. Likely doses would not cause cardiac
>depression in normal patients but, if strictly necessary, CPR could be
>administered until medical help arrives.
>
>Environment:
>1) Heavy metals: By definition, the fluxes will remove heavy metal
>oxides from the solder and components to form heavy metal salts. These
>will be removed in the Vigon solution. This solution, and the filter
>cartridges, are therefore hazardous waste and must never be disposed of
>by normal channels without prior recovery of the heavy metals. As the
>solution is used for long periods, because of their unique process, the
>metal concentration may rise to such levels that the solution dragged
>out may contain enough to contaminate the first wash water, depending on
>the cleaning machine design. It is therefore essential to check that
>this water, too, is acceptable for disposal according to the local
>regulations
>2) pH: Most water companies accept waste water with a pH between 6 and
>8.5 or 9 (check your local regulations). You are required to ensure that
>anything you send to waste is within tolerance. The solution most
>certainly isn't. If your waste water is consistently alkaline, some
>types of sewage pipes could be damaged, causing leaks that would be
>health hazard for the local population.
>3) Biodegradability: everything organic is biodegradable, given enough
>time and the right conditions. Ideally, we want biodegradation to be as
>rapid as possible. Given enough oxygen, there is no reason to believe
>that Vigon A-200 would not aerobically degrade rapidly, which is good.
>However, is there enough oxygen? Many treatment plants for either
>industrial or publicly owned run at the limit of their oxygenation
>capabilities. If it is insufficient, suddenly adding large quantities of
>Vigon solution with a relatively high concentration of organic matter
>with C-3 or higher molecules may overload the capabilities of the plant.
>Check with your effluent/hazardous waste disopsal chain.
>4) VOC: Vigon is a volatile organic compound: check with your local
>authorities whether you require a scrubber in your ventilation system
>before discharge to the air.
>
>I'm sorry to be a prophet of doom but, from the info given in posts
>here, it would seem that some users may have been ill-informed. I'm
>therefore putting the church back where it belongs, in the middle of the
>village.
>
>I put into service the first Vigon A-200 system in Switzerland. I was
>very impressed by its performance, better than other saponifiers I
>tried. It's damn good, in fact. However, I was unimpressed by the fact
>that the importer had not complied with Swiss labelling requirements nor
>given my client any H&S advice. However, at the time, it was a new
>product and I assumed that the appropriate compliance would follow. With
>this experience, I do know what I'm talking about, so please give me a
>little credit and, if you use the product, make sure you use it well and
>safely. You can only be satisfied if you wish to go the saponification
>route.
>
>Best regards,
>
>Brian
>
>PS PLEASE spell my name correctly: flattery will get you nowhere :-)
>
>-------------------------------------------------------------------
>--------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail
>to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-------------------------------------------------------------------
>--------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|