Unfortunately, the fab house said that they did this before. After trying
(and failing), they said that they didn't want it anymore. The Sales guy is
forcing them into trying some more. Obviously, we're not buying these
boards from them. I hope they're not listening... we haven't told them
yet.
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: Hinners Hans M Civ WRALC/LUGE
[SMTP:[log in to unmask]]
Sent: Friday, March 08, 2002 12:21 PM
To: [log in to unmask]
Subject: Re: [TN] CIC... ONCE AGAIN
Hey Jim,
I'm curious. Did you hear, "no problem . . . " from the Fab house
or the
Sales guy? You're giving me flashbacks, Sales booked a new order
(with
material we haven't even played with) and us Fab Engineers developed
a new
process on the fly - for a quick turn! Fortunately, my lamination
stuff
usually required only minor tweaking. I feel your pain.
Hans
Gunship Motto: "You can run . . . but you'll only die tired."
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Electronics Engineer
Warner Robins - Air Logistics Center (WR-ALC/LUGE)
226 Cochran Street
Robins AFB GA 31098-1622
mailto:[log in to unmask]
Com: (478) 926 - 5224
Fax: (478) 926 - 4911
DSN Prefix: 468
-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]]
Sent: Thursday, March 07, 2002 4:07 PM
To: [log in to unmask]
Subject: [TN] CIC... ONCE AGAIN
Remember all of those e-mails back in November regarding MLBs with
CIC
layers? Well, it's time again... We went ahead and designed a CIC
board,
mainly because our present board house said "no problem, we do it
all the
time". Well, he fell on his face and now, 3 months after placing
the order,
he can't deliver. Obviously, he has little, if any, experience with
CIC.
His problem is "...inserting the invar material into the copper
tanks kills
the solution and provide no plating". He is suggesting gold plating
the
vias first, then copper plating. Has anyone ever heard of this
before? Is
this a viable solution? Anyway, we're now looking for a new board
supplier
who HAS experience with CIC. Any recommendations? This is a
prototype run
of 5 boards only.
Thanks again for all your help,
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to
[log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources &
Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|