I have had good results with 100% solids silicone coatings dispensing
with a PVA system.

Jon Moore
TRW

>>> Graham Naisbitt <[log in to unmask]> 04/15/98
12:01pm >>>
Hi Technetters

Can anyone provide information about experiences with new solventless
coatings on Selective Coating equipment.

Have you been obliged to change application heads or use special
dispense
pressures? We are trying to help out some customers who are receiving
conflicting information and would appreciate any TechNetter input

Kindest regards

Graham Naisbitt - Concoat Ltd
Alasan House
Albany Park
Camberley, Surrey GU15 2PL UK

Tel: +44 (0) 1276 691100
Fax: +44 (0) 1276 691227

E-Mail: [log in to unmask]
Regards, Graham Naisbitt

Concoat Ltd
Alasan House, Albany Park
CAMBERLEY GU15 2PL
UK

Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227

email: [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2