I use a thermally conductive epoxy from Epoxy Technology (930-4) It
is a two part system but has excellent strength.
______________________________ Reply Separator _________________________________
Subject: ASSY: thermocouple adhesive
Author: [log in to unmask] at Internet
Date: 1/9/97 12:32 PM
Can anyone recommend an easy to use, one part instant adhesive for attaching
thermocouples to BT epoxy and FR-4 PCBs (for thermal profiling work)? I
remember others using a Loctite product in the past but I don't remember the
type. The adhesive only has to last about 10 runs through the oven.
Thanks
Don Foster
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************