   I am currently venturing into the world of pcb metallic finishes.  I have acquired some pcb's with immersion gold on them and have met with what seems to be limited success.  I was wondering if there are any tricks of the trade for processing these style boards thru a conventional SMT/Wave solder process?  If a different formulation other than 63/37 solder paste is recommended? and who it stacks up to the OSP coatings?


	Stephen Weldon
	Manufacturing Engineer
	Diagnostic Instrument Co.
	[log in to unmask]


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2