Ed Gavin wrote:
>
> Trying to elimenate pinholes(many) and blowholes(some)
>
> Situation:
> Through hole technology, 0.062 double side PCB
> OA 20% solids flux, .905 spec gravity
> Wave Temp - 500*F Preheat top side temp of 190*F
> Speed 4.5 FPM
>
> Have tried baking 215*F for 2 hours
> Have microsectioned board, copper in holes looks good
>
> Believe some components could be contaminated, could this cause the
> condition?
> Looking for suggestions
>
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]> *
> * with <subject: subscribe/unsubscribe> and no text in the body. *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
> ***************************************************************************
If components are contaminated,you should find the defects at the same
locations on the board.Maybe your board is contaminated.
Try to visually examine your boards for organic contamination and run
some bare boards through tht wave.
Gaby
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|