Hi Jason!
No, I've not done anything special with stencils I've ordered with round 0402
pads.
I normally get a 6-mil thick stencil, and check the box on the order form to
compensate the apertures to Industry Standards...
I've never had board with round wave solder pads, so I couldn't say for sure
how they would work. Then again, I've never tried wave soldering a 0402
either...something tells me I would be having other problems before I even got to
wave...like epoxy deposition.
Tom, I've got the picture up on my page at:
http://www.stevezeva.homestead.com and look at Round 0402 Pads...
-Steve Gregory-
> Thanks for the info Steve.
>
> Are there any special considerations needed when setting up the stencil
> apertures?
>
> Do you see any problems wave soldering these pads?
>
> Thanks
> Jason Lineback
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------