If immersion silver has such thorny issues then how did it ever get
approved by Bellcore? I will tell you, the evidence file presented by
Lucent was overwhelming!
Best regards
Lee
J. L. Parker Ph.D.
JLP Consultants LLC
(804) 779 3389
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Monday, December 18, 2006 9:06 PM
To: [log in to unmask]
Subject: Re: [TN] iNEMI Hi rel Pb-free finish report
Wayne,
First, you mean electrochemical migration, not electromigration. The
latter happens inside joints because of metal movement as a result of a
voltage potential and a high enough temperature.
Second, George Wenger and others at Lucent and people at Nortel (in
Harlow, England; RTP, North Carolina, USA and Belleville, Ontario,
Canada) did extensive studies on the stuff and didn't see issues. And I
know Lucent used boatloads of the stuff (and maybe still do). I expect
George will weigh in after he does some reading of that link you kindly
provided.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: December 18, 2006 2:50 PM
To: [log in to unmask]
Subject: [TN] iNEMI Hi rel Pb-free finish report
In this report (dated 12/1/06) there are several cautions about
Immersion Ag due to electro-migration issues, particularly in sulfurous
environments.
I know that UL recently "de-criminalized" ImAg, primarily based on IPC
pressure. Why hasn't iNEMI?
Can anybody recommend a paper which explains the severity of this
electro-migration issue with respect to ImAg?
Thanks,
Wayne Thayer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from
your system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|