Currently we are designing a board thicker than normal with small
holes.
The board is a 10 layer board, 082" thick, and uses 13.5 mil
drilled/plated holes.
The board is large ~ 13 x 16" in size. It is HASL. During component
assembly it will see 2 IR processes and a wave. We are specifying
the board as IPC Class 2. It will be used in high end computer
product. Reliability is very important.
In light of the above I have several questions for this distinguished
group:
1. Considering the 6 to 1 aspect ratio, using conventional FR-4 will
the design above have reliable plated through holes?
2. We are considering specifying that the FR-4 be of Tg greater than
170 Deg C. The hope is that this will improve hole relaibility. The
problem is that this will add significant cost to the board. Is it
necessary to do this?
3. The design is dense so that we cannot grow the hole significantly.
We are considering permitting hole breakout of 1 mil, so that the
holes can be drilled larger. Is this a reliability risk?
4. Are there other alternatives (not so expensive) to improve hole
reliability?
I would appreciate any feedback.
Thanks,
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|