Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Thu, 14 Oct 1999 08:40:26 +1000 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Hi Jim
You got good feed from Alain, Earl and Kelly .
That is from the fab side of the story .
You can double edge this (coupon) tool ;
if you integrate to fab coupon (bare board) also your troublesome component
mountings (say caps).
Than you can on the same coupon analyze metalography of joints ;
use them for cycling tests ;
comparative shear tests (process stability on the same/different parameters
[say different effects of various cooling profile scenarios]).
The population (pads/component) you can alter say with any new bare board
revision ;
that way you can plan to target your various woes (say cap pad geometry's) .
Obviously you parallel check your field as well , say cycling your coupons
will give you warning way ahead before it hits you = you can walk to MD
office and tell him he'll have a problem with this batch in 2 years or so
time,
because of this and that = supply service fellows with more clever
alternative before the tsunami in on them .
Concurrent engineering can be warped to limitless scapes ; often you need to
step back to see it .
Something about the trees and forests............
cu
Paul Klasek
http://www.resmed.com
-----Original Message-----
From: West, Jim [mailto:[log in to unmask]]
Sent: Thursday, 14 October 1999 0:23
To: [log in to unmask]
Subject: [TN] Specifying test coupons
Hi all,
Thanks to all that responded to my earlier test coupon question. I have a
few more question, how do you specify test coupons? What do I tell the
board layout guy? What do I tell the board house? Does everyone have test
coupons on all boards or only multilayer? Any good advice on how to specify
would be great!
Thanks,
Jim West
Manufacturing Engineer
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|