Steve,
Room Temperature Vulcanizing silicone.
I could not venture a source for the material that would be appropriate for
your use.
A word of caution though - I have a recollection of a very good friend of
mine (Hello Gene!) telling me that these materials become conductive at
high frequencies. I through this out there for what it is worth!
Joseph Webb
TET/Halco
################################################################