Subject: | |
From: | |
Date: | Fri, 16 Feb 1996 16:40:00 EST |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
A strong consideration for not using 1/2 ounce copper on internal
layers, is that you only half the width of copper to make a
connection at the barrel of plating. Possible problems. Be careful.
May not be reliable.
Norm Einarson
|
|
|