Wow. Never saw it except after multiple drops.
Bev
RIM
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Thu Jun 11 18:15:46 2009
Subject: Re: [TN] Corner ball pad cratering
That may be the case sometimes that pad cratering will occur just from the reflow process. We have some reason to suspect that it could occur later, due to some unique mounting of mechanical components, the size of the PCB (the potential for deflection), and when the defect seems to show up in the test process.
Genny
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*
Sent: June 11, 2009 3:33 PM
To: [log in to unmask]
Subject: Re: [TN] Corner ball pad cratering
Hi Genny,
Bythe time you can underfill, you already have pad cratering-so this does not help.
Why pad cratering?
Remember, 'pad cratering' results from a number of factors coming together. Those factors are: 1) SAC solders are about 40% stiffer generating higher forces on cooling; 2) SAC solders creep significantly slower and thus do not provide stress relief on cooling; 3) the delta-T between solder solidification and the glass transition temperature, Tg, doubles for SAC-solders thus doubling the thermal expansion mismatch and the resulting stresses; 4) for some PWB base materials the fillers and curing agents used to make the resin RoHS-compatible make the resin more brittle with less cohesive strength.
Solution Options: 1) reduce cooling rate from soldering to no more than 1.5°C/sec; 2) use PWB base materials with higher Tg; 3) increase solder joint thickness between component and soldering pad; and 4) my favorite, go back to environmentally friendly SnPb solder.
Werner
-----Original Message-----
From: Genny Gibbard <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, 11 Jun 2009 4:09 pm
Subject: [TN] Corner ball pad cratering
Hello all,
If you have identified a BGA with corner ball pad cratering, what would be your suggestions to correct this condition?
Our thoughts:
1. We plan to evaluate our handling processes to reduce/remove excessive flex/strain occurring around this part 2. We plan to evaluate corner bonding or underfilling for the BGA.
Which=2
0do you feel would be the best direction to go? Do you have other suggestions?
Thanks in advance for all your help
Genny
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|